Dear Technetters,

Recently we had a problem with some smt flashmemories on our assembled
boards.  After reflow, but probably before, we noticed a crack on top of the
component.
we presume that its a condensation problem but we're not sure. Sounds
familiar?


Lon weffers

Matas Electronics

----------------------------------------------------------------------------
----