Please don't use that etchant.  It is recommended for
a big hunk of copper - but is not recommended for
electroplated copper deposits such as are on printed
wiring boards.

The attack to the copper can and does mask the
presence of cracks and other problems

Hydrogen Peroxide/Ammonium Hydroxide is the
etchant to be used on printed wiring boards for
copper evaluations

Susan Mansilla
Robisan Laboratory

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2