TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 29 Sep 1998 15:35:09 GMT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Noel Cherowbrier <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Noel Cherowbrier <[log in to unmask]>
Content-transfer-encoding:
7BIT
In-Reply-To:
Organization:
Tecan Components Ltd
MIME-Version:
1.0
Parts/Attachments:
text/plain (38 lines)
Does anybody have any technical data for comparing standard screening
can capabilities to that of Metalised Plastics screening
qualities/capabilities.

I am interested in looking at producing our
screening cans in a suitable plastic material  and plating them.
Whilst the RF Shielding capabilities would probably not be as good as
standard Copper tin plated cans it may be sufficient for our puroses
whilst at the same time reduce our costs.  Before we go ahead with an
expensive programme to measure this it may be that somebody has
already done so.

Does anybody have any ideas please.

Thanks

Noel Cherowbrier
Tecan Components Ltd
Tecan Way
Weymouth
Dorset
England  DT4 9TU

Tel +44 1305 765432
Fax +44 1305 780194

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2