The company I work for wants to use DLO/RHH flexible wire ( very similar to
welding wire) in the electric control panels we build. The UL inspector has
informed me that in order to do so we have to tin the ends of the wire (AWG
1/0 and larger) he said that some of the panel shops he covers use a solder
pot to tin the wire. I contacted Kester and inquired about the best solder
and method to use. The engineer that replied suggested I contact IPC forum
and inquire. So here is my question. What is the recommended solder and if
needed flux to use to tin the ends of this flexible wire?
Douglas Minniear
Lewis and Clark Machine
P.O. Box 615
501 Lottery Ln.
Hines, Oregon 97738
541-589-1330 cell
541-573-3044 fax
[log in to unmask]
INTERNET SECURITY STATEMENT
This electronic mail message, including attachments, is a confidential
communication exclusively between Lewis and Clark Machine, Inc. and the
intended recipient(s) indicated as the addressee(s). It contains information
that is private and may be proprietary or may be covered by legal
professional privilege. If your receipt of this transmission is in error,
please destroy all copies and notify this firm immediately by phone or reply
to this transmission.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|