Tim,
Since this assembly probably wont last very long, the easiest thing to do is to use Sn-Pb solder to "tin" the ENIG on your PCB, clean your site then place your flip chip on the site and send it into a "peaky" Sn-Pb reflow cycle....
That should form theinterconnects you need without all the other issues that ACF/ACA entail and would probably last as long...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tim Mack
Sent: Thursday, May 08, 2008 1:21 PM
To: [log in to unmask]
Subject: [TN] ACF/ACA Flip Chip Assembly
Hello TechNet,
Since tomorrow is Friday I thought I better get this out today.
I have a bare Si flip chip with plated gold bumps that I need to attach to
an ENIG finished FR-4 PCB (the PCB can be changed if ENIG is a bad idea).
My plan is to use Anisotropic Conductive Film/Adhesive (ACF/ACA) to produce
the interconnects. The chip itself has a 3x4 bump array with a 275 µm
pitch.
Does anyone here know of vendors for this material? Past experience do's or
don'ts? Any info would be appreciated.
Thanks,
Tim Mack
Research Engineer
NDSU Center for Nanoscale Science and Engineering
<http://www.ndsu.nodak.edu/cnse> www.ndsu.nodak.edu/cnse
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|