TECHNET Archives

September 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Jeff Meier <[log in to unmask]>
Date:
Wed, 5 Sep 2001 09:27:59 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (23 lines)
We currently do most of our soldering using water soluble flux that we
wash off in an in-line wash system.  We occasionally have to hand solder
parts that are considered not water washable so we use no clean flux
that leaves a flux residue on the board.  Our customers are requiring no
flux residue to be left on the boards.  We currently try to remove
residue by scrubbing and cleaning by hand which is very labor intensive
and probably does not totally remove residue.  I am looking for
alternate cleaning method suggestions that have been successful that you
have used.  Has anyone had much luck with the HFE solvents that are
freon alternatives and how difficult were they to implement use of.
Thanks,
Jeff Meier

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2