Good afternoon everyone,
I am currently reviewing a tombstoning problem that we are having with the
capacitors listed below. We are seeing this problem on two separate
electronic assemblies but only with this component style. We place 40 caps
per array and approx. 3 - 5 of them tombstone. Both assemblies go through
the SMT process and they both are using a Panasonic ECH-U1H152JB5 and
ECH-U1C153JB5 film capacitors. The placement of the capacitors pre-reflow
is centered correctly between the pads. But of course post reflow -
tombstone!
Any thoughts, ideas, or experiences with this part would be helpful.
Thanks in advance for your help.
Rich Lasko
Badger Electronics
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------