Trace wisth entering SMT pads should not be bigger than 80% of the pad width.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Thursday, January 13, 2011 5:24 PM
To: [log in to unmask]
Subject: Re: [TN] Trace Widths Entering SMT
I think you just took this topic a different direction.
IR boards most certainly do not heat evenly. But the original question
about a blanket rule about maximum .020" trace (or replacing a .050
w/ 3 .020 traces) didn't sound related to that problem.
Uneven copper distribution, parts sinking heat, large copper areas..
you can't ignore those. Trace sizes can effect balanced heating, but
they fall a little further down the list, and there's a lot more to it than
simply spec'ing a maximum width.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|