TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bill Kasprzak <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Kasprzak <[log in to unmask]>
Date:
Mon, 12 May 2008 10:33:45 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (157 lines)
Gosh, with all due respect, I'm sure the equipment is using the Galden 
fluid for vapor and that drag out if any is minimal. No environmental 
concerns as far as I can tell.

I think vapor phase will be the comeback kid in the years to come because 
of the even distribution of heat. (We do not have any lead-free soldering 
issues here)

What I'm really talking about out is how inconsequential our impact on 
global warming compared to the enormous volcanic eruption in Chile. Some 
of the photo's are incredible. Maybe Steve can post them. I think they are 
available from the UK's Daily mail website.

What's happening right now in Chile is a huge environmental disaster and 
no one, no laws, no regulations can do anything about it. It just shows 
how inconsequential we really are.




Bev Christian <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
05/12/2008 09:26 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Vapor phase






Ioan,
Ask the supplier what is the global warming potential of the materials
they are proposing as the thermal transfer material.  Then you have to
decide if you can live with the answer.

Also, RF cans with small holes can be problematic.

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, May 12, 2008 9:24 AM
To: [log in to unmask]
Subject: [TN] Vapor phase

Dear Technos,

 

I would like to get your expert opinion on the latest developments in
the vapour phase technology. The last time this topic has been discussed
here this was still an environmental hazard.

 

Here's the latest sales pitch:

 

Dear Convection Oven Users:

With Energy Costs Skyrocketing, You have a cheaper, efficient, and a
better yield Alternative!!

Low Operating Cost, 110 Volt Machine, Run Lead and Lead Free
Sequentially!! 

High Yield, Run your Lead Free Boards at 230 Degrees Uniform Temperature
Distribution, No Circuit Board Delamination, Uses Environmentally
Friendly Teflon 2 Liquid No Hazardous Florocarbons!

 

The questions are:

*       Are the advantages real, should I prefer vapour phase over
convection in day by day reflow operations, from the technical point of
view?

*       Would the technology finally be environmentally friendly?

 

Thanks,

 

Ioan

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from 
your system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be 
unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2