TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 6 Sep 2011 09:40:08 -0400
Reply-To:
Message-ID:
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (30 lines)
Hi,

 I have some small bobbins I make where magnet wire is wrapped on a bobbin
terminal then hand soldered. The magnet wire has a solder-able (heat
stripped) insulation and it solders much better with an iron tip of 450C. (I
normally use iron tips at 350 or lower.

 Has anyone seen fluxes designed for this temperature? I would like to use a
no clean. I get a log of flux "charring" as terminals are soldered, I would
like to see that residue reduced.

Thanks,
Bob K.


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2