I can cheat too.
I can do a cross section of a single row, put it face down on the x-ray
table and use maximum magnification.
I am pretty sure that a good X-ray equipment will show something.
But then- i can always use my microscope and get a much better picture.
Gaby
----- Original Message -----
From: "Werner Engelmaier /*" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, February 16, 2008 6:16 PM
Subject: Re: [TN] X-Ray equipment
> Hi Vladimir,
> The fractures that these X-rays show are not wide open.
> I know IPC strips things off/out, but I think the image below should get
> through to at least you.
>
>
>
>
>
>
>
>
>
> Werner
>
>
>
> **************
> The year's hottest artists on the red carpet at the Grammy
> Awards. Go to AOL Music.
>
> (http://music.aol.com/grammys?NCID=aolcmp00300000002565)
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|