TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 9 Jul 2008 16:08:17 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Tontis <[log in to unmask]>
Subject:
From:
Ted Tontis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<003c01c8e203$fcacee30$f606ca90$@net>
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (19 lines)
5) How would you know if you have inner layer shifting? 

Take a look at IPC 2221A, table 12-1 and figure 12-14 show registration
coupons that could be used.

http://members.ipc.org/committee/drafts/7-11_d_Coupons.pdf

Ted T 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2