TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, bob wettermann <[log in to unmask]>
Date:
Thu, 9 Apr 2009 12:05:43 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=iso-8859-1
From:
R Sedlak <[log in to unmask]>
Parts/Attachments:
text/plain (46 lines)
Bob:  Remember there is no such thing as an oxide-free Tin surface, that is more than a few seconds old, and the older the surface, the thicker the oxide.  I suspect strongly that bond strength is going to very related to oxide thickness, no matter the adhesive composition.
It might even be worth considering some sort of oxide removal, even abrasive, before applying adhesive.
Rudy Sedlak
RD Chemical Company

--- On Thu, 4/9/09, bob wettermann <[log in to unmask]> wrote:

From: bob wettermann <[log in to unmask]>
Subject: [TN] Friday Theorizing
To: [log in to unmask]
Date: Thursday, April 9, 2009, 8:17 AM

Dear Technetters:

Has anyone done any adhesion testing of a 2um tin-electrocoated surface (copper carrier) to FR-4? How about a 0.100um tin electrocoated surface? Can someone theorize on which might give better adhesion using a 2-part epoxy?

Regards

 Bob Wettermann
BEST
PH 847-767-5745

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



      

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2