The corner crack data is very well depicted in IPC-RB-276 Figure 7 and Table
10 and is perhaps clearer than the examples shown in IPC-A-600.  As RB-276 is
the document from which IPC-A-600 takes its info, it should be used to as the
controlling document.

The answer to your question is that B cracks cannot extend into the plating
for Class 2 and 3   

Phil Hinton 
hintpwb1 @aol.com 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2