I would try one or two Yag shots instead, Pd and Kovar excellent targets for 1um wave
Ingemar
-----Original Message-----
From: Mike McMahon [mailto:[log in to unmask]]
Sent: den 16 mars 2001 00:59
To: [log in to unmask]
Subject: Re: [TN] Soldering
Asahi Glass makes something called a 'Sunbonder' to complement their Cerasolzer line of Indium-based solders.
It's a manual soldering system incorporating ultrasonics; both tip temperature (to 450C) and ultrasound power are controllable. I've used one with a number of Indium alloys (not yours, though) for fluxless soldering to metallized glass. The ultrasound seems to promote wetting to otherwise difficult materials. There are automated systems around too.
Asahi's distributer is:
Bellex International Corp
Wilmington, De
(302) 761-9886
http://www.bellexinternational.com/sunbonder.htm
Hope this helps.
Michael McMahon
Three-Five Systems
>>> [log in to unmask] 03/15/01 01:23PM >>>
Hello Fellow Netters,
Here's a recipe for a soldering nightmare. We're developing a
process that involves the following materials, but not having very good
success with attaining an 'acceptable' solder joint.
Lap soldering a .4 mil dia platinum wire to the top of a .040" dia
kovar post using indium solder (60% indium/40% lead). Additional info: the
kovar post has a nickel coat 200 micro inches, then 30 micro inches of hard
gold plating.
One issue: indium solder does not wet to tip of iron and platinum
wire (tip temp is at 670F)
Second issue: If we use zinc chloride as a fluxing agent, the end
solder is better, but we would rather stay away from using this flux (too
corrosive).
Does this challenge anyone out there? We'd appreciate any and all
feedback.
Process Control Supervisor
[log in to unmask]
Industrial Scientific Corp.
www.indsci.com
voice 412.490.1884
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|