TECHNET Archives

February 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Diaz, Lourdes" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 24 Feb 1999 15:37:04 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Technet,

Has anyone done a study on the correlation of board reliability vs. the
number of components replaced by board?
We have a certain amount of boards we will like to convert into another
product.     The conversion requires component to be deleted and/or added.
Quantity of components to be deleted/added varies from 3 to 75 depending on
the configuration we want to go to.    85% of the components to be replaced
are SMT discrete components the rest are TH capacitors, (x5 leads)
transformers.   These boards had been through 2 SMT processes(components top
and bottom) and wavesolder.    One is a 8 layer board, 0.062" thick, SOBC,
wet film soldermask, 5.51" wide by 8.17" long.     The other one is a 2
layer board, 0.062" thick, SOBC, wet film soldermask, 7.44" wide by 11.995"
long.
How much rework can one do to the board and still feel confident that the
product won't fail in the field?

Thanks,

Lourdes Diaz
Manufacturing Engineering
Milgo Solutions, INC
[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2