TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
john maxwell <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Wed, 5 Nov 1997 12:24:42 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (38 lines)
Tamir,
Run an experiment to see if the problem is related to board moisture
absorption of adhesive over temperature during cure. Take a reasonable
quantity of boards where one would expect to see failures, bake out half of
the boards prior to assembly at 125 degree C for 8 hours and then run both
sets of boards with only chips attached to see if solder shorting occurs.

Section portions of the boards under the components from the board bottom
up and look for bubbles or voids between the two different lots.

If it still occurs then examine the adhesive cure profile to make sure that
the adhesive does not exceed manufacturer's recommended maximum temperature
during cure. I have seen incidence where there is an exothermic reaction
between the resin and hardner during excessive temperature cure that
results in out gassing or bubbling of the adhesive.

Again section portions of the board from the bottom up to look for voids
under the part.

Regards,


John Maxwell
Please contact me off line at [log in to unmask] if there are any further
questions.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2