IF reflowing the internal MCM joints is a genuine concern, and you are
going to reflow attach these with other devices rather than separately,
your best bet is probably a "Pb-free" paste. These use SAC type alloys
melting in the 217C range.

More important than alloy though you need minimum superheat on
processing to limbo under the 230C peak so find a decent supplier.
However this implies virtual zero delta T in your process.
Also you need to be aware of the implications for changing your solder
type, it would be a good idea to review the surfaces finishes etc with
your prospective supplier.

If that doesn't work there maybe 1 or 2 other possibilities but these
will cost.
Example: Separately attaching the MCM would allow internal Sn63 as now,
but you could use a lower MP solder [than Sn63] for device attach.

Regards

Mike Fenner

Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Sergey Ermolin
Sent: Tuesday, December 16, 2003 4:04 PM
To: [log in to unmask]
Subject: [TN] high-temperature alloy and process for a multi-chip module


Hi.

I am desinging a multi-chip module. In my desing, two off-the-shelf IC's
in TQFP packages are mounted on an FR-4 PCB. This board has a Land Grid
Array footptint on the bottom and will be soldered to the motheboard
using a standard reflow process with Sn63Pb37 alloy. What alloy and
temperature profile would you recommend for assembling the multi-chip
module itself? The chips on the module were not designed to withstand
more than 230 deg C and are normally soldered using the same Sn63Pb37
alloy...

Thank you for your help...

Regards,

Sergey Ermolin
Dust, inc
2560 9th Street, #218
Berkeley, CA 94710
510/225-2137

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2