Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Fri, 6 Dec 1996 12:14:39 -0700 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vW5w5-0000XnC; Fri, 6 Dec 96 13:27 CST |
Resent-Message-ID: |
<"xEUPL1.0.M2O.qE7go"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Fri Dec 6 15: |
33:46 1996 |
Cc: |
|
X-Mailer: |
Windows Eudora Light Version 1.5.2 |
Message-Id: |
|
Parts/Attachments: |
|
|
arlon clte
1. Dk 2.94
2. dissapation factor .0025
3. cte x=10ppm, y=12ppm, z=40ppm
4. tg = 300 c
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|