TECHNET Archives

January 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 27 Jan 1998 14:41:48 +0900
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Motoyo Wajima <[log in to unmask]>
Subject:
From:
Motoyo Wajima <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset=iso-2022-jp
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
Mr. Engelmaier!
"I"stands for interstitial.
Regards,
Motoyo Wajima


Werner Engelmaier <[log in to unmask]>  $B$5$s$O=q$-$^$7$?!' (J
>Hi Jae-heun,
>I sure have not come across the acronyms "BVH" and "IVH" before; I take it
>that VH stands for via hole, B perhaps for blind, but what is "I"?
>I do not know of any reliability studies on blind vias. As a first step and
>until more definitive information is available, I would apply the information
>in IPC-D-279, "Design Guidelines for Reliable Surface Mount Technology Printed
>Board Assemblies", Appendix B, to blind vias. Considering the construction,
>the loading on blind vias during soldering processes will be significantly
>less than for PTVs, and therefore the minimum copper plating thickness is most
>likely defined by functional or manufacturing requirements, not reliability
>issues.
>
>Werner Engelmaier
>Engelmaier Associates, L.C.
>Electronic Packaging, Interconnection and Reliability Consulting
>7 Jasmine Run
>Ormond Beach, FL  32174  USA
>Phone: 904-437-8747, Fax: 904-437-8737
>E-mail: [log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>

***********************************************
Motoyo Wajima
General Purpose Computer Division,Hitachi,Ltd.
1 Horiyamashita
Hadano-shi,Kanagawa-ken,259-13 Japan
E-mail:[log in to unmask]
Fax:+81-463-88-2935
***********************************************

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2