We just installed a rubber ESD floor which works great.  The installer did
recommend that the old tiles be removed, though.  It costs about $6.50/sq.
ft. for removal of the old tiles and installing the new.

Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879



        -----Original Message-----
        From:   Howard Watson [SMTP:[log in to unmask]]
        Sent:   Wednesday, October 10, 2001 10:55 AM
        To:     [log in to unmask]
        Subject:        [TN] ESD flooring ideas.


        Dear TechNetters,

        Our PCB assembly area is being consolidated to another building, and
I have the opportunity to request some type of ESD floor coating over an
existing non-ESD tile flooring.  What are your opinions on the best, most
reliable, and of course cheapest, method of ESD flooring?  I am thinking
that removing the existing tile would not be a cost effective alternative.
We are moving out of a facility that had no ESD flooring, so improvements
should be easy to achieve.  Thanks for the assistance.

        Best regards,

        Howard Watson
        Manufacturing Engineer
        AMETEK/Dixson

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2