Hi Scott - If I was a betting man, my guess is that Steve "poured" some
solderballs on the assembly and took a picture of a "perfect" defect.
That's a whole bunch easier than trying to place it (at least with my eyes
too).
Dave
"Post, Scott E" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/07/2012 07:55 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Post, Scott E" <[log in to unmask]>
To
<[log in to unmask]>
cc
Subject
Re: [TN] Need image of solder ball shorting a device
If Steve placed that solder ball then he's definitely got better eyesight
and dexterity than me.
Scott Post
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, March 06, 2012 3:10 PM
To: [log in to unmask]
Subject: Re: [TN] Need image of solder ball shorting a device
Nice job, Steve!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, March 06, 2012 1:37 PM
To: [log in to unmask]
Subject: Re: [TN] Need image of solder ball shorting a device
Hi Scott,
Albeit staged, how would this one work for you?
http://stevezeva.homestead.com/SolderBall.JPG
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Post, Scott E
Sent: Tuesday, March 06, 2012 10:31 AM
To: [log in to unmask]
Subject: [TN] Need image of solder ball shorting a device
I'm putting together some internal training materials on ANOVA,
regression,
and DOE and I'm making up an example scenario along with some fake data
for
the students to work through. Can someone send me a picture of a small
solder ball (maybe a mid-chip solder ball from a resistor) that got loose
and lodged between a pair of QFP/SOIC/BGA leads causing a short? I have
plenty of pictures of mid-chip solder balls from back when we were using
rectangular paste apertures, but I don't have a picture of one getting
loose
causing a short.
Thanks,
Scott Post
P.O.U. 0000-001E-0CTC
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
****************************************************************************
************ Note: If the reader of this message is not the intended
recipient, or an employee or agent responsible for delivering this message
to the intended recipient, you are hereby notified that any dissemination,
distribution or copying of this communication is strictly prohibited. If
you
have received this communication in error, please notify us immediately by
replying to the message and deleting it from your computer. Thank you.
****************************************************************************
************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
****************************************************************************************
Note: If the reader of this message is not the intended recipient, or an
employee or agent responsible for delivering this message to the intended
recipient, you are hereby notified that any dissemination, distribution or
copying of this communication is strictly prohibited. If you have received
this communication in error, please notify us immediately by replying to
the message and deleting it from your computer. Thank you.
****************************************************************************************
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|