TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Black, Paul" <[log in to unmask]>
Date:
Wed, 24 Nov 2004 15:34:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
The issue is not Tg but Td.  Some higher Tg materials actually perform
worse than lower Tg materials.  It is important develop a test program
to validate your lead free process with specific base materials.
Laminate manufactures offer some variety of thermally stable materials
targeting lead-free, but these are used at a premium.  If your lead-free
process can be supported by existing base materials, than that is best
economic solution.  The test program will provide the feedback needed.

Please contact me off-line if you need specific information on alternate
base materials and Td for lead-free.   

Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
  76 Technology Drive - POB 1890
    Brattleboro, Vermont 05302
      Voice: 802.257.4571.21 Fax: 802.257.0011
           http://www.vtcircuits.com
 

-----Original Message-----
From: Black, Paul [mailto:[log in to unmask]] 
Sent: Wednesday, November 24, 2004 3:08 PM
To: [log in to unmask]
Subject: [TN] FR4 and Lead free

Hi Tech Gurus,

As people talk more and more about Lead free, I keep hearing that
standard FR boards might not be able to take the extra heat required for
a reliable Lead free solder joint. The problem is that I keep hearing
the word MIGHT. I have not heard that this is definitely true and, if it
is true, I have not heard anyone offer a cost effective solution. So, I
am asking the many experts on this forum, will standard FR4 be able to
handle the higher excursions (particularly, let's say, for a 7" X 9",  8
layer, double-sided SMT, .062" 5/5 board) associated with Lead free
solder paste? If not, what would be the most cost-effective offering
(i.e. high Tg FR4)?

Thank you, 
Paul Black 
Manufacturing Engineer 
Kronos 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2