TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"Myug C. Chu" <[log in to unmask]>
Date:
Tue, 21 Jul 1998 13:01:08 +0900
Content-Type:
text/plain; charset="us-ascii"
X-To:
Kathy Palumbo <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Myug C. Chu" <[log in to unmask]>
Parts/Attachments:
text/plain (80 lines)
Hi Young and One:

Please do check this out.  The technology looks great.

MCC

>Johannes,
>
>I have tried this type of stencil.  It was made by a company in Canada
called KJ Marketing.  It worked extremely well.  The material is laser cut,
and as a result of the heat from the Laser the walls of the apertures are
perfectly smooth.  The release of paste was outstanding.  It performed as
well or better than a pure nickel stencil.
>
>Alignment was made easy due to the ability to see through the stencil.
>
>The material can be melted down and used again, and it does not stretch as
much.
>
>You should try it out yourself and see what you think.
>
>Thanks,
>Kathy Palumbo
>> ----------
>> From:         Johannes Sivula[SMTP:[log in to unmask]]
>> Sent:         Tuesday, June 30, 1998 4:18 AM
>> To:   [log in to unmask]
>> Subject:      [TN] Polyimide See Thru Stencils for Printing Solder Paste
>>
>> Polyimide See Thru Stencils for Printing Solder Paste
>>
>> Following mail was posted by  Russ M on June 23, 1998 at 11:27:37: to
>> http://www.smtnet.com/smt_forum/smt_mail.html
>>
>>           Has anyone seen/used these yet?  They seem to have lower
coefficient of friction  for release of paste and less wear and  tear as
well as  conforming to the board  better     (plastic has better memory than
stainless). Also there is no  mesh  so a larger image can be put in a
smaller stencil size. But, the best is that you can see through  the stencil
for manual and semi-automatic printer alignment and  reduce set up and
changeover times.
>>           Anyone familiar with these?
>>           How long do they last?
>> --------------------------------------------------------------------------
>> -
>> ----------------------------------------------------------
>> Any comments ?
>> brs, Johannes
>>
>>
>>
>> This type os stencil is available from:
>> KJ Marketing Services
>> 115-30th St.
>> Toronto, Ontario, M8W 3C1
>> Phone: (416) 252-1061
>> Fax: (416) 253-1687
>> email: [log in to unmask]
>> Web Site: www.kjmarketing.com
>> Regards John Parsons Circuit Graphics Ltd.  [log in to unmask]
>>
>>

CSS Asia Co., Ltd.
Tel: 82-2-523-8810
Fax: 82-2-523-1483
E-Mail: [log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2