What's really ironic about Bismuth being considered, is the fact that it's
usually obtained as a by-product of lead mining!
Go figure...
-Steve Gregory-
> Re: Bi,
>
> I am a little surprised to see Bi as a leading candidate. At a seminar I
> attended, the subject of Bi in solder was discussed. I thought I heard that
> Bi was meeting resistance, especially in Europe, because the environmental
> issues with it were worse than the lead it was replacing. Not being a
> chemist, I don't know which is worse from a landfill toxicity viewpoint -
> 2%Bi or 37%Pb. It is also quite possible I misunderstood what was said about
> Bi! Is Bi as a component of solder an environmental concern?
>
> Thanks.
>
> =========================
> Bob Barr
> Manufacturing Engineering
> Formation, Inc.
> =========================
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|