TECHNET Archives

November 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jonathan A Noquil <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 8 Nov 2000 18:36:54 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (30 lines)
Hello Technetters, esp those deal with SMT, am just wondering
why my solder joint become powdery. I mounted SOIC-8 on a Nickel Au
finished
PCB using 63 Sn /35Pb/2Ag solder paste then subject it to PRCL reliability
test
the solder joint become powdery and i can removed the component
softly. Any explanation for this? I mean why it become powdery. I really
checked the
solder joint after reflow and It was good.

Same thing i did on BGA, i put bumped wafers on steam aged environment
and the solder balls after exposure become powdery.

Any theoretical or actual explanation on this

thanks

Jonathan Noquil
Package/Design (R&D)
Fairchild Semiconductor

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2