TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Knowles, Ed" <[log in to unmask]>
Date:
27 Sep 1996 12:51:27 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)

(This is my second attempt at sending this.  I'm still trying to 
figure out how to get mail out of here.  Sorry if it's a repeat 
question for some, but I didn't get any responses.)

Does anyone have information on the affect on reliability in a thermal 
cycle environment of gull wing leaded devices that are not completely 
on the pad (up to 25% side overhang).  For Class 3 hardware, J-STD-001 
allows up to 25% overhang, a value that was determined by pull test to 
not degrade reliability significantly.  I have seen one paper that 
suggested greater than 50% decrease in thermal cycle fatigue life with 
leads 25% off the pad (actual testing, no analysis performed).  
Reliability prediction models show a decrease in fatigue life with 
decreasing solder area under the lead, however, when microsectioning 
leads I found very little difference in solder area between a 25% and 
0% overhang.  The only significant difference was the absence of a 
fillet on the overhanging side.
Thanks.

Ed Knowles
Lockheed Martin Astronautics
[log in to unmask]
phone 303-977-3560

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2