TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Mon, 26 Nov 2007 10:30:28 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
Short term immersion in water typically does not contribute to any
significant moisture adsorption in most PWBs. It is the longer term
exposure to humidity that causes PWBs to eventually reach saturation.
However, there are always exceptions. Simply get a precision scale and
weigh a number of pwbs prior to and after wash and record the delta. The
scales can be leased for very reasonable cost and many scale providers. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, November 26, 2007 9:45 AM
To: [log in to unmask]
Subject: [TN] PCA washing

Hi Technos,

 

I need to set the process of aqueous washing on our in-line machine and
have a BIG preliminary question:

 

How to make sure that my boards are properly dried at the end of the
machine? Is the absence of water on the surface of the board, including
under the parts, a thorough indicator? Is it possible that residual
humidity be found inside the laminate?

 

Thanks for your help,

 

Ioan


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2