Hi Ralph! Can you provide more information on what the customer
considers/experienced "corrosion" and what type of use environment he/she
was talking about?
Dave Hillman
Rockwell Collins
[log in to unmask]
Ralph Richart <[log in to unmask]>@IPC.ORG> on 06/08/2000 11:55:26 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to Ralph Richart <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] still confused
We have answers....
So I had a long talk with my customer this morning to provide input
based on the invaluable advice from you all.
I said - "is there a specific reason for choosing 3-8u" of immersion
gold over tin/lead solder?"
He said - "absolutely, the gold provides corrosion resistance, the gold
does not"
I said - "even such a thin amount - only 3-8u"?"
He said - "definitely, all we need is the coverage, the thickness is
irrelevant"
Is this true?
Needless to say, we are rebuilding the parts as we speak. Rework sounds
difficult to say the least, although I may try to come up with some
scheme for fun as they have a bunch of boards that are no good right
now.
thanks for all the help.....
ralph
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|