TECHNET Archives

November 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 16 Nov 2009 11:04:32 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (60 lines)
Hi Inge,
Certainly have. This is not new, and it is not very surprising.
You may be interested in my White Paper on how to design PCBs for reiability given Pb'free soldering.
Werner


-----Original Message-----
From: Hernefjord Ingemar <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Nov 16, 2009 3:22 pm
Subject: Re: [TN] Microvia reliability vs Lead free



 


any relationships are described, one of which is a Curtiss-Wright report. They 
ave exposed identical boards to SnPb soldering/repair and compared with same 
or SACs, and found a significant difference in time to failure. 
                  
                                      1st thermal cycle to failure
                    As Received             6 x 230 Celcius         6 x 260 
elcius
Mean                        788                 443                 4

That is a dramatic change in via failures.  We have seen some failures recently 
n ordinary double sided FR-4 boards, which were exposed to several heat 
xposures in conjunction with electrical testing. Far from 260 Celcius, think 
nly 125 Celcius. If we got microvia issues with only 125 C, what if we use 260 
 (e.g. repeated repair)?
Has anyone seen any signs of via failure due to increased heat exposure in 
ractice?

nge
--------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
dditional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2