Barrie
I do not see how it would improve things - or am I missing something?
A cleanliness check using some form of ionic tester is only a monitor of the
performance of your process and only measures ionic contaminants that it can
get at. It cannot detect non-ionics that have been proven to be a major
contributor to circuit failures. New ionic test systems don't really do it
any differently or necessarily any better. I do concede however, that a
static tester will do the job far quicker.
So it would surely be more appropriate, as you move into finer pitch/width,
COB devices and greater miniaturisation, to take another look at the
potential reliability of your end product. This would be better done using
either new SIR testing or Ion Chromatography testing specs. / systems that
are now available.
Regards,
Graham Naisbitt
[log in to unmask]
WEB: http://www.concoat.co.uk
CONCOAT Ltd
Alasan House, Albany Park
CAMBERLEY GU15 2PL UK
Tel: +44 (0) 1276 691100 Fax: +44 (0) 1276 691227
----- Original Message -----
From: Candeas, Barrie <[log in to unmask]>
To: <[log in to unmask]>
Sent: 07 February 2000 14:58
Subject: [TN] Ionic Contamination Testing
> I am looking to update my Omega-Meter 600R for a tester that is more
current
> and able to test complex, densely populated PWAs. Any experience with new
> testing gear would be appreciated.
> Barrie Candeas
> General Dynamics
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|