I can't tell for the 093 boards because we haven't assembled any yet.
That's why I was wondering if anybody can tell me which web thickness and
angles are preferable.
And I am not afraid of having trouble breaking the parts, I am afraid of
having trouble with boards going in the wave and not beeing strong enough
because of the V-GRROVE resulting in "warpage"...again with .093"....
At 10:23 PM 98/04/06 EDT, GuitarBud wrote:
>Do the parts break out nicely?
>
>Do you have lengths of 3 or more inches that are scored and still break
>nicely?
>
>Frank
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
>################################################################
>
>
>
Annie Laberge
Ingenieure Qualite
Les Systemes Electroniques Matrox
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|