TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], "lduso - Diamond-MT.com" <[log in to unmask]>
Date:
Fri, 17 May 2013 08:28:19 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Message-ID:
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (73 lines)
Hi Lloyd,

I'm sorry I didn't make it clear. I'm referring to water soluble masks
before wave solder, not conformal coating....

Steve Gregory

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lduso -
Diamond-MT.com
Sent: Friday, May 17, 2013 7:25 AM
To: [log in to unmask]
Subject: Re: [TN] Water soluble masks compatible with closed-loop water
treatment systems

Tough to put into practice. With masking you want to get the masking
material off before the coating has completely cured to minimize lifting
and peeling. The washing machine could damage that uncured coating. Plus
the coating is covering the masking so the water will not touch the
masking to dissolve it until the coating is removed from it first. I
tried it with parylene and we had to pick holes in the film so the water
could access the masking then go back and trim off the excess after the
masking dissolved and we were left with a "tent" of film

Re-usable boots are ideal but could be costly when you have many
different style/sizes of connectors.

Like we tell all our customers, cheapest way to coat something is leave
off all the connectors!!

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com


On Fri, May 17, 2013 at 9:08 AM, Steve Gregory <
[log in to unmask]> wrote:

> Morning all,
>
> Continuing on with the masking thread, I know Techspray has a water 
> soluble mask that is supposed to be compatible with closed-loop water 
> treatment systems, are there any others out there?
>
> Any pros/cons of using them?
>
> As always, thanks in advance!
>
> Steve
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2