We take masking off after the coating has come to a tack free state, but
before cure. That way we can touch up any coating that comes up prior to
cure. I suspect that the coating is getting under the spray fixtures and
the cured coating adheres it in place.
Doug Pauls
Jeff Smith
<jeffs@PENTAGON-E
MS.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
03/08/2007 02:10 [TN] CC fixture issue
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Jeff Smith
<jeffs@PENTAGON-E
MS.COM>
We have a customer using a masking fixture for their conformal coating
process. They're running into an issue with the cover adhering to the
board
after curing. The fixture is made from 6061 Aluminum, and the coatings
being
used are:
Arathane 5750 A/B with a Cellosolve acetate Thinner
Aptek 2512
Humiseal 1B31 with Humiseal 521 Thinner
We make thousands of these fixtures a year and haven't run into this
problem. We're exploring possible solutions, so I thought I'd post a
couple of
questions:
1) Does the board need to remain in the fixture until fully cured?
2) is there an issue with these specific coatings?
Thanks!
Jeff Smith
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|