TECHNET Archives

June 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Watson, Howard August" <[log in to unmask]>, [log in to unmask]
Date:
Tue, 2 Jun 2015 19:09:30 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Vladimir Igoshev <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
MIME-Version:
1.0
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (35 lines)
It's definitely done thing on top of the board. To be more certain,‎ we'd need the board for analysis.

Regards,

Vladimir

Sent from my BlackBerry 10 smartphone on the Rogers network.
  Original Message  
From: Watson, Howard August
Sent: Tuesday, June 2, 2015 18:56
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] PCB blob defect

Hi all,

My PCB fab knowledge is limited, and a very unusual defect was discovered (too late) in assembly. I'm wondering if anyone has seen something like this before, or has an idea what this could be. The blue color seems noteworthy to me. This is for IPC class III, space. I will return this to the fabricator, but I wanted to get educated in case there is a debate regarding the cause. Thanks for your help!

Steve put the pictures here:

http://stevezeva.homestead.com/Howards_Blob.jpg

http://stevezeva.homestead.com/Howards_Blob_close.jpg
Howard A. Watson

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2