Fri, 1 Jul 2005 08:43:46 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (94 lines)
Hi Brian - would the ditchwitch "tool"  have applicability for the removal
of paralyene conformal coating? :)

Dave Hillman
Rockwell Collins
[log in to unmask]




             Brian Ellis
             <[log in to unmask]>
             Sent by: TechNet                                           To
             <[log in to unmask]>         [log in to unmask]
                                                                        cc

             07/01/2005 08:37                                      Subject
             AM                        Re: [TN] Semi chip removal tool
                                       wanted

             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
                Brian Ellis
             <[log in to unmask]>






As it's Friday,
http://www.ditchwitch.com/dwcom/Product/ProductView/10578 :-D

Brian

Ingemar Hernefjord (KC/EMW) wrote:
> Hi everyone.
> Anybody seen a good tool for removing silver epoxy mounted semiconductor
chips? Probably kind of electromechanical mini tool, but I have not found
any useful. Diamond high rpm tool is not good because you spread particles
all around. Shearing is seemingly best way. Today's method with sharp tool
and hammer is too primitive.
> Ingemar Hernefjord
> Ericsson Microwave Systems
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
>

--
______________________________________________
Please note new e-mail address [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2