Wet: Adhere, join, bond.... Not melt
-----Original Message-----
From: Kane, Amol (349) [mailto:[log in to unmask]]
Sent: Friday, June 02, 2006 10:11 AM
To: TechNet E-Mail Forum; Dehoyos, Ramon
Cc: [log in to unmask]
Subject: RE: [TN] BGA solder
Hi Ramon,
What do u mean by wet? Do you mean melt? ........What reflow profile was
used? If SnPb temperatures were used, then SAC balls will not reflow and
form a homogenous joint, which creates reliability issues........a sort
of a hybrid profile is needed to solder backward compatible BGAs using
SnPb solder.....depending upon the % of solder volume of SAC BAG to the
% of solder volume of SNPb on the pad, the SAC can melt anywhere from
210 to 215 degree C. the key is to hold it above that temp just enough
to melt all the SAC and dissolve it in the SnPb to form a homogenous
microstructure, but not to overheat the SnPb components
Wow! Haven't seen the Mixed BGA scenario....not yet atleast!
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Friday, June 02, 2006 9:55 AM
To: [log in to unmask]
Subject: [TN] BGA solder
Two experiences were shared with me and would like them to be
known for comments. In one instance a COTS BGA was used on a prototype.
It would not wet to SN63Pb37 after several attempts and profile
temperature increments It was found out that it had SAC 305 balls. Has
anyone experienced that SAC does not wet well with eutectic tin lead
solder paste? In another instance balls from SAC and Tin Lead were found
in the same BGA. Apparently solder balls were inadvertently mixed.
Ramon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|