TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Eric Christison <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 2 Oct 2001 05:49:42 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (118 lines)
Joe,

We use 5352R. They have others too which may suit your application better.
They should be able to advise you on this plus required equipment.

Regards,



> ERIC
> Do you know the the 3M part no# for this tape? I am very intrested to see
>  if
> it help with a problem i have
>
>
>
>    thankyou
>    JOE KEARY
>
> -----Original Message-----
> From: Eric Christison [mailto:[log in to unmask]]
> Sent: Monday, October 01, 2001 3:14 AM
> To: [log in to unmask]
> Subject: Re: [TN] Flex and Soldering
>
>
> We attach a flex to a ceramic substrate using a hot bar BUT using a 3M Z
> axis adhesive tape.
>
> The flex has very closely spaced pads and these were prone to shorting
>  when
> we tried hot bar soldering. We also found the adhesive gave a stronger
>  joint
> mechanically.
>
> However cycle time for hot bar - whether solder or ACF - is not that
>  good. I
> would suggest about 1 minute per joint and it is done manually although
>  a
> certain amount of automation is possible.
>
> One very large phone manufacturer told me the other week that they
> absolutley loathe the hot bar process. A yield hit of 8% on a million
>  phones
> a month gets your name in the corporate spotlights...
>
> Hope this helps,
>
>
>
> > Technet,
> >
> > Does anyone have any guidelines for soldering flex circuit directly to
>  a
> > PWB?  We currently connect it mechanically and with a connector, but
> > were toying with the idea of direct solder attach.
> >
> > Any experience, do's and don't, especially horror stories, appreciated.
> >
> > Thanks......DT
> >
> >
> >
>
>
>
> Eric Christison
>
> --------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
>  in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
>  >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>  additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> --
> -----
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
>  in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
>  Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases
>  > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>  additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>  ext.5315
> --------------------------------------------------------------------------
> -------
>

Eric Christison

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2