Hi Dewey,
No, HTE/E3, does in fact have better ductility than E1, and its 3-sigma outliers give you more than the 2% elongation you can get for 3-sigma product of E1.
Werner Engelmaier
-----Original Message-----
From: Whittaker, Dewey (AZ75) <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 29 Apr 2005 09:02:22 -0700
Subject: Re: [TN] Copper Foil Spec "HTE"
I always thought it stood for " Hell, That's Equivalent ", because of the
variations in measuring techniques; baked or not baked; conditioned;
effective ductility vs. thickness, so on so forth.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Parsons
Sent: Thursday, April 28, 2005 4:03 PM
To: [log in to unmask]
Subject: [TN] Copper Foil Spec "HTE"
Hi All,
Is it;
a) Close to Friday and I just can't think of the answer
b) Old age affecting my memory
c) I have never come across this spec and just don't know what it
means!
I have a requirement for copper foil to "HTE type E class 3"? I suspect
that there is nothing fancy about this but what is "HTE" ?
Regards
John Parsons
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|