At Alpha Metals, L0 means no halide in the formula;
this is true for liquid fluxes and solder pastes.
UP78 is REL1, and it passes AgCrO4 paper.
We consider it a Bellcore compliant paste, but it's still REL1.
It is REL1 because it's formula contains halide. Take a look at
our technical bulletin.

UP78-OSP is REL0, it has no halide in it's formula.  We don't
add any halide to it.  Any trace halide in UP78-OSP is from
trace halide contaminants in the raw materials, very, very tiny.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2