TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 29 Aug 2007 10:00:40 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Dennis Fritz <[log in to unmask]>
Parts/Attachments:
text/plain (36 lines)
 
In a message dated 8/29/2007 2:23:11 A.M. Eastern Daylight Time,  
[log in to unmask] writes:

Hi  Leo,
I have some data about hydrolysis for a glassfiber reinforced PWB  type
that is similar to FR-4. Two diagrams on tensile modulus and  tensile
strength vs. immersion in stem and water vs time up to 1,000 hs.  Can
send offline if  you are  interested.
Inge


I have the same interest - physical properties of laminate with changes in  
humidity.  My interest is in vibration performance of military boards, and  we 
have determined that laminate stiffness definitely plays a role. However, we  
would also like to know if "wet - Somalia" versus "dry - Saudi Arabia" 
locations  also affects vibration performance.  Thanks in advanced. 
 
Dennis Fritz
SAIC, Inc (Crane Naval Weapons Depot - Indiana).  



************************************** Get a sneak peek of the all-new AOL at 
http://discover.aol.com/memed/aolcom30tour

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2