TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Thu, 20 Apr 2006 12:19:09 -0400
Content-Disposition:
inline
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Wayne Thayer <[log in to unmask]>
Subject:
From:
Wayne Thayer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (51 lines)
The pads do seem to be contaminated with something.  What was the
surface finish of the boards prior to soldering? OSP?  Immersion tin?
ENIG?

>>> [log in to unmask] 4/20/2006 11:42:01 am >>>
I received some PWB photo from my customer which they claim the
present
of "Solder Resist(Clear Color)" on the Solder Pad thus preventing the
solder from wetting. In your opinion, what's that clear color layer of
substance that is preventing it from wetting? Is it really solder
resist?
Picture:
http://img115.imageshack.us/img115/6089/untitled3or.jpg
http://img126.imageshack.us/my.php?image=untitled16ut.jpg

This PWB is coated with Green Color Solder resist,if it is really
solder
resist, shouldn't it be Green color instead of Clear? I am puzzle why
the
resist turn clear instead of Green when adhere to the solder pad. Can
someone teach me?

Sorry if you feel this is a noob question as I am new.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2