     Hi,
     
     I wont to clarify regarding the max weight for double side reflow, i 
     ment that there is a ratio between the surface energy and gravity, one 
     of the way to masure the adhesion is to test when does a melt droplet 
     is seperated from the solid surface, and with the use of Young-Dupre 
     equation you can calculat the surface energy.


______________________________ Reply Separator _________________________________
Subject: Re: Max weight in DSR
Author:  	Victor Li <[log in to unmask]> at INTERNET
Date:    3/4/97 1:00 PM


Is there such a ratio between surface tension and gravity force ? 
Where can I find it?
     
Thank you very much.
     
Best regards,
     
Victor
     
     
     
On Thu, 3 Apr 1997, Tamir Ben-Shoshan wrote:
     
>      Hello,
>      
>      Does anyone calculate the max chip's weight for double side reflow in 
>      
>      more accurate way then comparing the surface tension with the gravity 
>      
>      force.
>      
>      Thanks, Tamir 
> 
> *************************************************************************** 
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
> *************************************************************************** 
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
> * with <subject: subscribe/unsubscribe> and no text in the body.          * 
> *************************************************************************** 
> * If you are having a problem with the IPC TechNet forum please contact   * 
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
> *************************************************************************** 
> 
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2