Paul,
I can give you some ideas on the cause:
Pinholes in solder mask typically have a few possible sources, depending on the application and type of the solder mask. Screen printed solder mask can have pinholes from plugged screens. Photoimagable solder mask can get pin holes from bad artwork or debris on the artwork or exposure frame.
Dan Blattman
Taiyo America
-----Original Message-----
From: Stolar, Paul W [mailto:[log in to unmask]]
Sent: Wednesday, January 08, 2003 12:32 PM
To: [log in to unmask]
Subject: [TN] Pinholes
I am seeing pinholes in the solder mask of a board.
Any words of wisdom about the cause? Or Dispensation?
Paul Stolar
Materials Engineer
Baker Atlas
713-625-5376
<font size="2">---------------------------------------------------<br>
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e<br>
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet<br>
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)<br>
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest<br>
Search the archives of previous posts at: http://listserv.ipc.org/archives<br>
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315<br>
-----------------------------------------------------<br></font>
<font size="2">---------------------------------------------------<br>
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e<br>
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet<br>
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)<br>
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest<br>
Search the archives of previous posts at: http://listserv.ipc.org/archives<br>
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315<br>
-----------------------------------------------------<br></font>
|
|
|