TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Anil kher <[log in to unmask]>
Date:
Fri, 10 Jun 2011 05:14:37 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Message-ID:
Subject:
From:
"Wenger, George M." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
<013401cc2741$653ebe30$2fbc3a90$@com>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (231 lines)
What happens if the nickel is 1.5 to 3 microns?

Regards,
George
George M. Wenger
Senior Principal Reliability / FMA Engineer
Andrew Corporation - Wireless Network Solutions
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 Office (732) 309-8964 Mobile
E-mail: [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Anil kher
Sent: Friday, June 10, 2011 3:38 AM
To: [log in to unmask]
Subject: Re: [TN] Black Pad?

We found an easy method to determine Black Pad. Check under an XRF with
Gold/ nickel calibration.
If no black pad the nickel will be ~ 3 to 5 microns. Wherever the nickel
goes down to 1/1.5 microns and gold shows same - sure u hv black pad.
Of course - that is how black pad is formed. But well in the hole - a cross
section will be better.
Its also the layout which causes black pad - we observed some pads with very
low nickel and the same would not solder. Nearby bigger pads showed adequate
Ni and soldered well.
My 2 bits
Anil Kher

-----Original Message-----
From: Gerry Gagnon [mailto:[log in to unmask]] 
Sent: Thursday, June 09, 2011 11:19 PM
Subject: Re: Black Pad?

Me too. It looks like oxidized nickel which will not wet.
 
> Date: Thu, 9 Jun 2011 09:12:00 -0700
> From: [log in to unmask]
> Subject: Re: [TN] Black Pad?
> To: [log in to unmask]
> 
> I'm with Steve on this one...
> 
> Paul
> 
> Paul Edwards
> Process/Quality Engineering
> Surface Art Engineering
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Thursday, June 09, 2011 6:59 AM
> To: [log in to unmask]
> Subject: Re: [TN] Black Pad?
> 
> Hi Gary,
> 
> I got your pictures this morning, and have them posted now:
> 
> http://stevezeva.homestead.com/Joint_1.JPG
> 
> http://stevezeva.homestead.com/Joint_2.JPG
> 
> http://stevezeva.homestead.com/via.JPG
> 
> Although the pictures show some non-wetting happening, it's difficult to
see
> what exactly is going on.
> 
> You say that the component side seems fine, it's just when you're trying
to
> wave solder is when you see the problem. Maybe you have thin gold, and
when
> the boards were fresh, the SMT was able to solder fine. But then after the
> boards went through reflow, the underlying nickel oxidized so badly that
> solder wasn't able to wet?
> 
> Steve
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Robinson
> Sent: Wednesday, June 08, 2011 4:46 PM
> To: [log in to unmask]
> Subject: [TN] Black Pad?
> 
> We have noticed a problem only on ENIG boards in our WAVE process that
looks
> similar to Black Pad but do not know how to identify or where to begin to
> find a resolution to the problem. We were hoping an expert may have
> experience in seeing this problem. Here are some facts -
> 1. Black residue is on the vias and thts on the solder side. Please see
the
> attached images.
> 2. Component Side SMT Parts do not exhibit the same problems.
> 3. Boards are processed PbFree - SAC305, Pacific 2009m No Clean Water
Based
> flux
> 4. THTs will not wet after residues appear (for touch up process)
> 5. Blowholes appear to accompany the defect but are not always present.
> 
> Thanks for your help in advance.
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
>
============================================================================
==
> 
> This email and any attachments thereto may contain private, confidential,
and
> privileged material for the sole use of the intended recipient. Any
review, copying,
> or distribution of this email (or any attachments thereto) by others is
strictly prohibited.
> If you are not the intended recipient, please contact
[log in to unmask]
> immediately and permanently delete the original and any copies of this
email and
> any attachments thereto. 
> 
>
============================================================================
==
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
 		 	   		  

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2