TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Date:
Thu, 4 Mar 2010 11:36:02 -0800
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Paul,

 

It's the parts that cannot go through the wash.

 

KennyB

  _____  

From: Paul Edwards [mailto:[log in to unmask]] 
Sent: Thursday, March 04, 2010 11:45 AM
To: TechNet E-Mail Forum; Ken Bloomquist
Subject: RE: [TN] Conformal Coat Over No-Clean Flux

 

BM_BEGINKen,

Is it the parts that can't go through the wash or you can't clean No-clean
off in your in-line?

Paul

Paul Edwards
Surface Art Engineering


-----Original Message-----
From: TechNet [ <mailto:[log in to unmask]> mailto:[log in to unmask]] On Behalf
Of Ken Bloomquist
Sent: Thursday, March 04, 2010 11:21 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat Over No-Clean Flux

This dialogue is great so far but one big part of my question is missing. I
cannot clean these solder joints with anything except spot cleaning. They
cannot go through our in-line wash. My understanding is that spot (bench)
cleaning is never a good idea as a final clean.

I understand that testing is required and I'm prepared to do that but just
wanted to get a feel for successes other people have had coating urethane
over no-clean.

By the way Inge, I'm not trying to cut corners by putting on no-clean pants
;-)

Thanks,

KennyB





______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2