TECHNET Archives

October 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Leo Higgins <[log in to unmask]>
Date:
Tue, 7 Oct 2003 09:04:23 -0700
MIME-Version:
1.0
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Roland Jaquet <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Leo Higgins <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
Roland,
    Try these sources:

www.polymet.com    North Attleboro, MA  USA
www.ametekmetals.com  Wallingford, CT   USA


Regards,
Leo Higgins


-----Original Message-----
From: Roland Jaquet [mailto:[log in to unmask]]
Sent: Tuesday, October 07, 2003 3:56 AM
To: [log in to unmask]
Subject: [TN] Copper/Molybdenum/Copper used for PWB heatsink ?


Dear Ladies & Gentlemen TechNetters.

One of my client is seeking a suppliers for Copper/Molybdenum/Copper used
for PWB heatsink

Is there any within US or Europe?

Thank you for your help

Best regards

Roland

www.PCBspecialist.com www.TechnoSphere.ch Jaquet Roland Consultant 14 ch de
Vers 1228 Plan-Les-Ouates, GENEVA Switzerland [log in to unmask] tel: fax:
mobile: 41228800405 41228800409 41792033723

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2