We've done it, but if the cause of the problem was solderability then it
probably will not help. If you are correcting a preheat problem or
solder temp problem, it can help.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Stokes
Sent: Wednesday, August 21, 2002 4:12 PM
To: [log in to unmask]
Subject: [TN] Re-Waving electronic assemblies
Anyone out there have any information or input into the acceptability of
putting an electronics assembly back through a wave process a second
time as part of a rework process?
Please advise,
Kevin Stokes
Quality/Reliability Manager
Kimball Electronics Group - Jasper, Indiana
------------------------------------------------------------------------
--------- Technet Mail List provided as a free service by IPC using
LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To
temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to [log in to unmask]: SET Technet
Digest Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|