Sort of related question - I am experimenting with a batch cleaner for WS
flux removal. I am using DI water for the wash and rinse cycle. I have
not "blown off" the excess water, just placed the assembly in a dry
chamber. The assemblies have "water-spots" on them. Do you have any
experience with this problem? I heard of an additive but can not readily
find information or suppliers of such a product.
Thanks for your help.
Douglas A. Hooper, Sr.
Luminescent Systems, Inc.
[log in to unmask]
-----Original Message-----
From: Dewey Whittaker [SMTP:[log in to unmask]]
Sent: Thursday, October 28, 1999 10:24 AM
To: Hooper; TechNet
Subject: RE: [TN] inline cleaner / RMA flux
"Collins, Graham" wrote:
> Good Day Technet!
>
> I'm looking for recommendations today. We use RMA flux and currently
use a
> batch cleaner (semi-aqueous). I'm looking at a big upswing in volumes
> (YAY!), which will obviously mean more cleaning - so I'm looking into
making
> the leap to an inline cleaner.
>
> Does anyone in the RMA world have recommendations for particular
machines,
> and/or cleaning additive? We are using Bioact EC-7R in our batch
cleaner.
>
> My other restrictions? Due to budget I'm looking for a used machine,
and
> please don't suggest that I change from RMA flux. I'd love to change
> fluxes, but to even suggest it to one particular customer causes them
to
> start to twitch and pop prozac like they are M&Ms...
>
> As always, thanks for any help!
>
> Graham Collins
> Process Engineer,
> Litton Systems Canada, Atlantic Facility
> (902) 873-2000 ext 6215
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following
text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
> 847-509-9700 ext.5365
> ##############################################################
Graham,If you would like to call me off-line I will try to help you
out.There
are a
lot of things to consider and it is important to understand the
variables.
Dewey
--
Dewey Whittaker
Honeywell -- Air Transport Systems Division
US Mail: P.O. Box 21111 MS: M16A2 Phoenix AZ 85036
Phone: +1 602 436 436-2766
NSFnet: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|