TECHNET Archives

October 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sun, 27 Oct 2002 12:32:33 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jack Crawford <[log in to unmask]>
Subject:
From:
Jack Crawford <[log in to unmask]>
X-cc:
"Jennifer Day (Jennifer Day)" <[log in to unmask]>, "Tino Gonzalez (Tino Gonzalez)" <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (72 lines)
Please don't shoot the messenger; just sharing industry consensus criteria. Steve, if your agreement is to accept to IPC-A-610 you need to consider the following and develop exception agreement with your customer if appropriate. As can be seen, the requirement to solder press-fit pins isn't new.

Based on the number of "you shouldn't" replies to Steve's posting, I find it unusal that I can't find any record of comment submitted to this criteria in the past seven years. 610 revision efforts are underway. Further, I don't remember discussion on this criteria at any of the approx. 40 Rev C development committee meetings. Now is the time for someone to step forth with some failure substantiation because of soldering or the committee likely won't consider changing the soldering requirement. Anyone with support of why it's necessary to solder would also be welcome to revalidate the existing requirement.

Criteria in IPC-A-610B pub Dec 94 and currently in Rev C pub Jan 2000:

6.9 Connector Pins - Press Fit Pins

Target - Class 1,2,3
* A 360° solder fillet is evident on the secondary side of the
assembly.
Note: Solder fillet or fill on primary side is not required.

Acceptable - Class 1,2
* Solder fillet or coverage (secondary side) is present on two
adjacent sides of the pin.

Defect - Class 1,2
* Less than two adjacent sides with solder fillet.
* Less than two sides soldered.
Defect - Class 3
* Less than four sides of pin contain solder.

Acceptable - Class 1
* Solder wicking is permitted above 2.5 mm [0.0984 in] on
sides of pins provided there is no solder build up which
interferes with subsequent attachments to the pin.
Acceptable - Class 2,3
* Solder wicking on sides of pins is less than 2.5 mm [0.0984
in], provided the solder does not interfere with subsequent
attachments to the pin.
Defect - Class 1,2,3
* Solder build up interferes with subsequent attachments to
the pin.
Defect - Class 2,3
* Solder wicking exceeds 2.5 mm [0.0984 in].

Comments need to be in the following format:
Name/company/phone & email so committee leaders can contact you for more info.
Paragraph/figure number being commented against:
Your recommendation:

Reason for requesting the change (substantiation):


Thanks to all for support of TechNet and the peer-consensus standards development process.

Cordially
Jack

Jack Crawford
Director, Professional Development and Assembly Technology
[log in to unmask]
847-790-5393
fax 847-504-2393

APEX 2003 March 31-April 2 Anaheim CA
www.goapex.org
IPC Printed Circuits EXPO March 25-27 Long Beach CA
http://www.ipcprintedcircuitexpo.org/

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2